Polymer
polypropylene
polymer
Structure
[*]CC(C)[*] |Sg:n:1,2,3::ht|
About
| Wikidata | Q146174 |
|---|---|
| Instance of | type of polymer |
| Polymer of | propylene |
| CAS | 9003-07-0 |
| ChEBI | CHEBI:53550 |
| EC number | 618-352-4 |
| ECHA InfoCard | 100.117.813 |
| DSSTox | DTXSID00872805 |
| MeSH | D011126 |
| Wikipedia | English, Dutch, German, French, Italian, Spanish, Persian, Russian, Japanese, Chinese |
| Scholia | Literature about this polymer |
| OpenAlex | Literature about this polymer |
Properties
| Property | Value | Conditions | Source |
|---|---|---|---|
0.9025 ± 0.0025 gram per cubic centimetre |
applies to part:
plastic foil
determination method or standard:
ASTM D1505
state of matter:
solid
temperature:
23 degree Celsius
uncertainty corresponds to:
measurement value interval
|
||
1.35 ± 0.50 gigapascal |
applies to part:
plastic foil
determination method or standard:
ASTM D638
uncertainty corresponds to:
measurement value interval
|
||
1.55 ± 0.50 gigapascal |
determination method or standard:
ASTM D638
fabrication method:
injection molding
uncertainty corresponds to:
measurement value interval
|
||
57.5 ± 2.5 Rockwell scale |
applies to part:
plastic foil
determination method or standard:
ASTM D785
temperature:
23 degree Celsius
uncertainty corresponds to:
measurement value interval
|
||
62.5 Rockwell scale |
determination method or standard:
ASTM D785
fabrication method:
injection molding
temperature:
23 degree Celsius
uncertainty corresponds to:
measurement value interval
|
||
162 ± 1 degree Celsius |
applies to part:
plastic foil
determination method or standard:
differential scanning calorimetry
uncertainty corresponds to:
measurement value interval
|
||
163 ± 1 degree Celsius |
applies to part:
injection molding
determination method or standard:
differential scanning calorimetry
uncertainty corresponds to:
measurement value interval
|
||
2.3 |
frequency:
1000 hertz
frequency:
1000000 hertz
frequency:
1000000000 hertz
temperature:
25 degree Celsius
|
||
determination method or standard:
ASTM D256
fabrication method:
injection molding
lower limit:
0.3 joule per cubic metre
temperature:
23 degree Celsius
upper limit:
0.5 joule per cubic metre
|
|||
0.6 ± 0.1 joule per cubic metre |
applies to part:
plastic foil
determination method or standard:
ASTM D256
temperature:
23 degree Celsius
uncertainty corresponds to:
measurement value interval
|
Polymers in this class
The 3 subclasses and instances of polypropylene in Wikidata, also those of its subclasses. Those without a page here link to Wikidata.
-
Purpolen®PP recycling
No CXSMILES in WikidataQ57272759
-
CELRe
No CXSMILES in WikidataQ118594126
-
Isotactic polypropylene
No CXSMILES in WikidataQ140403649